Issues in the Early Development Stage:
◆ Gate area prone to black streaks, yellow streaks, cracking, and sticking (especially for temperature-sensitive PET materials) due to cooling effects
◆ Long cooling cycle time
Solution:
◆ Resolved through conformal cooling channels
Advantages:
◆ Cooling cycle shortened by 10 seconds
◆ Smooth gate area on the product, free from defects such as cracking and sticking